Skip to main content
TPU · Flexible

Bambu TPU 95ATPUFilament Review & Print Settings

4.4/5

Bambu TPU compatible with AMS for multicolor flexible prints. Medium hardness.

Quick Specs

Brand
Bambu Lab
Material
TPU
Print temp
220-240°C
Bed temp
50°C
Speed
30 mm/s
Cost/kg
$35

Colors Available

BlackWhiteRedBlueClearGrey

Print Settings Guide for Bambu TPU 95A

Flexible TPU requires a fundamentally different approach than rigid filaments. Direct drive extruders handle TPU far better than Bowden setups — Bowden tubes cause buckling and inconsistent extrusion on soft materials. Nozzle: 220-240°C. Bed at 50°C — TPU adheres well to PEI at moderate temps. Print speed is the critical variable: 30 mm/s maximum — faster speeds cause the TPU to compress and buckle in the extruder path before it reaches the nozzle. Retraction: disable or minimize (0–1mm) — TPU rebounds elastically, causing underextrusion if retraction is too aggressive. Fan cooling at 50–100% for detail retention.

Why Choose Bambu TPU 95A

Bambu TPU 95A balances printability and mechanical flexibility better than most TPU options. Bambu Lab rates their TPU for consistent Shore hardness batch-to-batch — critical for functional parts like gaskets where compliance matters. TPU's chemical resistance to oils, greases, and many solvents makes it viable in industrial environments where rubber parts wear out. Abrasion resistance is significantly higher than rigid filaments. The predictable elastic recovery of quality TPU means printed springs and compression pads behave consistently across cycles, unlike cheaper formulations that creep under sustained load.

What to Print with Bambu TPU 95A

Bambu TPU 95A is the material for anything that needs to flex, grip, or absorb shock. Phone cases, tablet bumpers, protective covers for electronics. Gaskets, o-ring replacements, and custom seals for low-pressure applications. Shoe insoles, orthotic inserts, and ergonomic grips. Drone motor mounts that absorb vibration. Cable strain relief boots. Flexible hinges for boxes and enclosures. Tires for RC cars and robot wheels. The higher the Shore hardness rating, the stiffer the part — 95A is firm (like a shoe sole), 85A is more rubber-like, and 70A is very soft and stretchy.

Common Issues & Fixes

Buckling in Bowden tubes: switch to direct drive — this is the root cause of 90% of TPU failures. Stringing: lower temp 5°C, minimize retraction, reduce travel speed. Underextrusion: slow down further, check extruder grip, ensure filament is straight going into extruder. Elephant foot: raise Z-offset slightly — TPU squishes more than rigid filaments. Difficult removal from bed: let cool completely before removing; TPU contracts and releases cleanly. Inconsistent extrusion: TPU must be stored dry (absorbs moisture); dry at 50°C for 4 hours.

Notes

One of few TPUs compatible with AMS system. Slow print speeds.

Where to Buy Bambu TPU 95A

Find Bambu TPU 95A from Amazon and authorized resellers. Price comparison helps — filament costs vary by vendor, fulfillment location, and quantity. Check manufacturer storefronts for direct pricing and bundle deals.

PrintLog3D participates in the Amazon Associates program. Purchases through our links may earn a small commission at no extra cost to you.

Log your TPU prints in PrintLog3D

Track your actual settings for Bambu TPU 95A — nozzle temp, bed adhesion, slicer profile, and results. Build a settings history that tells you exactly what works.